Kerui andalusite brick is used in the first lining of various industrial furnaces. The refractoriness under load reaches a maximum of 1700℃ (3092℉). Andalusite brick can effectively improve the efficiency of high temperature industrial furnace.
| Indicator | MLUT-62 | MLUT-69. |
|---|---|---|
| Al2O3, not less, % | 62 | 69 |
| Fe2O3, not more than % | 1.3 | 1.2 |
| Open porosity, %, not more than | 17 | 19 |
| Compressive strength, N/mm2, not less than | 50 | 50 |
| Additional linear shrinkage at T=1500℃ and 2 hours exposure time, %, no more than | 0.6 | 0.6 |
| Softening onset temperature under 0.2 MPa load, ℃, not lower | 1600 | 1650 |
| Heat resistance (heating up to 1300℃ - water), heat change, not less than | 25 | 30 |
| item | RH-155 | RH-150 | RH-145 | RH-140 | RH-135 | RH-130 | |
|---|---|---|---|---|---|---|---|
| Al2O3, % | ≥ | 69 | 65 | 61 | 57 | 53 | 49 |
| Fe2O3,% | ≤ | 1 | 1 | 1.2 | 1.2 | 1.5 | 1.5 |
| TiO2, % | ≤ | 0.5 | 0.5 | 0.5 | 0.6 | 0.6 | 0.6 |
| Porosity, % | ≤ | 20 | 20 | 20 | 20 | 20 | 20 |
| Volumetric density, g/cm³ | 2.55~2.70 | 2.50~2.65 | 2.45~2.60 | 2.40~2.55 | 2.35~2.50 | 2.30~2.45 | |
| Compressive strength, MPa | 55 | 55 | 50 | 50 | 40 | 40 | |
| 0.2MPa softening temperature under load, ℃ | ≥ | 1700 | 1700 | 1650 | 1600 | 1520 | 1450 |
| Permanent replacement of heating line, % | 1500℃*2h ±0.2 | 1450℃*2h ±0.2 | |||||
| Creep rate (0.2MPa, 0-50h) / % | ≤ | 0.8 (1550℃) | 0.8 (1450℃) | 0.8 (1400℃) | 0.8 (1350℃) | 0.8 (1300℃) | |